We try for excellence, service the customers", hopes to be the most effective cooperation workforce and dominator company for staff, suppliers and shoppers, realizes price share and ongoing marketing for Pvb Film Catalogue, Pvb Film Price, Safety Glass Film, All of the time, we have been paying attention on all information to insure each product or service glad by our customers.
2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan Detail:

Medium Brown Pvb

Baizan color pvb film for architectural laminated glass.
Baizan can provides plenty of color film for customers choose with stable and accurate color.
production volume >12000t per year
Color pvb MOQ>5000 sq.m.
Payment term:TT LC DP
Delivery time :5-15days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Raw material inspection
In order to ensure the quality of products, we carry out strict inspection on raw materials, according to China national standards。
Detection of PVB resin powder

project volatile viscosity(20℃ 10%/S) Packing density(g/㎝3) Melt index(120℃  21.6kg g/10min) The fog degree(%) Light transmittance(%) Acid value(mgKOH/g) The hydroxyl content(Wt%) Butyl group content(Wt%) transparency

1.Sampling: after every lot of raw material arrive at factory, about 5kg samples will be taken from each lot.
2.Appearance test: white, fine and even, free from any impurity, free- flowing powder or particle.
3.Whiteness: take 2kg of the sample, add 1kg of plasticizer, mix well, extrude and shape the membrane, compare the color
4.The volatility:Weigh up the sample with an analytical balance and place it in a weighing bottle. Keep the bottle in the oven for 3 hours, with temperature 60℃(±1℃) . After taking it out, place it in the dryer for 20-30 minutes and then weigh it.
5.Viscosity:Add resin powder into a paper funnel, put a condensing tube in the 65℃ water bath for 1h, and when it is taken out and cooled to a constant temperature of 20℃±1, pour the sample into a scale cup, and record the time the first drop of solution reach to 50ml, which is the viscosity of the sample
6.Melt index:Weigh the powder and the plasticizer (1:3), adding the plasticizer first and the powder later. After adding it into the melting index flow rate meter, preheat for 4 minutes, add 21.6g weight and start extruding. After 3 minutes, cut off the first section, and then wait for 5 minutes before cutting the second section. The total weight of two sections will be the melting index value.

Customer usage scenarios

awf


Product detail pictures:

2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan detail pictures


Related Product Guide:

With our rich working experience and thoughtful companies, we have now been recognized as being a trustworthy supplier for a lot of global potential buyers for 2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan , The product will supply to all over the world, such as: Brunei, Belgium, Islamabad, By continuous innovation, we will present you with more valuable items and services, and also make a contribution for the development of the automobile industry at home and abroad. Both domestic and foreign merchants are strongly welcomed to join us to grow together.
  • Goods just received, we are very satisfied, a very good supplier, hope to make persistent efforts to do better.
    5 Stars By Pamela from Angola - 2017.08.28 16:02
    The customer service reprersentative explained very detailed, service attitude is very good, reply is very timely and comprehensive, a happy communication! We hope to have a opportunity to cooperate.
    5 Stars By Austin Helman from Suriname - 2018.11.22 12:28
    Write your message here and send it to us