Being supported by an highly developed and skilled IT group, we could offer you technical support on pre-sales & after-sales support for Color Pvb Film, Plastic Pvb Film, 0.45mm Pvb Film, Welcome to post your sample and color ring to let us produce according to your specification.Welcome your inquiry! Looking forward to building long-term cooperation with you!
2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan Detail:

Medium Brown Pvb

Baizan color pvb film for architectural laminated glass.
Baizan can provides plenty of color film for customers choose with stable and accurate color.
production volume >12000t per year
Color pvb MOQ>5000 sq.m.
Payment term:TT LC DP
Delivery time :5-15days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Raw material inspection
In order to ensure the quality of products, we carry out strict inspection on raw materials, according to China national standards。
Detection of PVB resin powder

project volatile viscosity(20℃ 10%/S) Packing density(g/㎝3) Melt index(120℃  21.6kg g/10min) The fog degree(%) Light transmittance(%) Acid value(mgKOH/g) The hydroxyl content(Wt%) Butyl group content(Wt%) transparency

1.Sampling: after every lot of raw material arrive at factory, about 5kg samples will be taken from each lot.
2.Appearance test: white, fine and even, free from any impurity, free- flowing powder or particle.
3.Whiteness: take 2kg of the sample, add 1kg of plasticizer, mix well, extrude and shape the membrane, compare the color
4.The volatility:Weigh up the sample with an analytical balance and place it in a weighing bottle. Keep the bottle in the oven for 3 hours, with temperature 60℃(±1℃) . After taking it out, place it in the dryer for 20-30 minutes and then weigh it.
5.Viscosity:Add resin powder into a paper funnel, put a condensing tube in the 65℃ water bath for 1h, and when it is taken out and cooled to a constant temperature of 20℃±1, pour the sample into a scale cup, and record the time the first drop of solution reach to 50ml, which is the viscosity of the sample
6.Melt index:Weigh the powder and the plasticizer (1:3), adding the plasticizer first and the powder later. After adding it into the melting index flow rate meter, preheat for 4 minutes, add 21.6g weight and start extruding. After 3 minutes, cut off the first section, and then wait for 5 minutes before cutting the second section. The total weight of two sections will be the melting index value.

Customer usage scenarios

awf


Product detail pictures:

2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan detail pictures


Related Product Guide:

We've got a highly efficient group to deal with inquiries from shoppers. Our purpose is "100% client fulfillment by our product high-quality, price tag & our staff service" and enjoy a superb reputation amongst clientele. With quite a few factories, we will provide a wide variety of 2018 Latest Design Pvb Glass Laminating Process - Medium brown BK104 / Medium brown BK103 – Baizan , The product will supply to all over the world, such as: Sao Paulo, Cologne, Japan, Now we are sincerely consider to grant brand agent in different areas and our agents' maximum margin of profit is the most important thing we care about. Welcome all of the friends and customers to join us. We are ready to share win-win corporation.
  • The company can keep up with the changes in this industry market, product updates fast and the price is cheap, this is our second cooperation, it's good.
    5 Stars By Elsa from Mecca - 2018.12.10 19:03
    Cooperate with you every time is very successful, very happy. Hope that we can have more cooperation!
    5 Stars By Clementine from Venezuela - 2017.10.13 10:47
    Write your message here and send it to us