Manufacturer for Pvb Interlayer - Medium brown BK104 / Medium brown BK103 – Baizan

Short Description:


Product Detail

Related Video

Feedback (2)

To be a result of ours specialty and service consciousness, our enterprise has won an excellent status between buyers all around the globe for Eva Film, Red Pvb, White Pvb, As we're moving forward, we continue to keep an eye on our ever-expanding merchandise range and make improvement to our services.
Manufacturer for Pvb Interlayer - Medium brown BK104 / Medium brown BK103 – Baizan Detail:

Medium Brown Pvb

Baizan color pvb film for architectural laminated glass.
Baizan can provides plenty of color film for customers choose with stable and accurate color.
production volume >12000t per year
Color pvb MOQ>5000 sq.m.
Payment term:TT LC DP
Delivery time :5-15days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Raw material inspection
In order to ensure the quality of products, we carry out strict inspection on raw materials, according to China national standards。
Detection of PVB resin powder

project volatile viscosity(20℃ 10%/S) Packing density(g/㎝3) Melt index(120℃  21.6kg g/10min) The fog degree(%) Light transmittance(%) Acid value(mgKOH/g) The hydroxyl content(Wt%) Butyl group content(Wt%) transparency

1.Sampling: after every lot of raw material arrive at factory, about 5kg samples will be taken from each lot.
2.Appearance test: white, fine and even, free from any impurity, free- flowing powder or particle.
3.Whiteness: take 2kg of the sample, add 1kg of plasticizer, mix well, extrude and shape the membrane, compare the color
4.The volatility:Weigh up the sample with an analytical balance and place it in a weighing bottle. Keep the bottle in the oven for 3 hours, with temperature 60℃(±1℃) . After taking it out, place it in the dryer for 20-30 minutes and then weigh it.
5.Viscosity:Add resin powder into a paper funnel, put a condensing tube in the 65℃ water bath for 1h, and when it is taken out and cooled to a constant temperature of 20℃±1, pour the sample into a scale cup, and record the time the first drop of solution reach to 50ml, which is the viscosity of the sample
6.Melt index:Weigh the powder and the plasticizer (1:3), adding the plasticizer first and the powder later. After adding it into the melting index flow rate meter, preheat for 4 minutes, add 21.6g weight and start extruding. After 3 minutes, cut off the first section, and then wait for 5 minutes before cutting the second section. The total weight of two sections will be the melting index value.

Customer usage scenarios

awf


Product detail pictures:

Manufacturer for Pvb Interlayer - Medium brown BK104 / Medium brown BK103 – Baizan detail pictures


Related Product Guide:

We always continually offer you by far the most conscientious customer service, and the widest variety of designs and styles with finest materials. These attempts include the availability of customized designs with speed and dispatch for Manufacturer for Pvb Interlayer - Medium brown BK104 / Medium brown BK103 – Baizan , The product will supply to all over the world, such as: Russia, Macedonia, Pakistan, With the technology as the core, develop and produce high-quality merchandise according to the diverse needs of the market. With this concept,the company will continue to develop merchandise with high added values and continuously improve items,and will present many customers with the best goods and services!
  • It is not easy to find such a professional and responsible provider in today's time. Hope that we can maintain long-term cooperation.
    5 Stars By Rosalind from Singapore - 2017.09.30 16:36
    Perfect services, quality products and competitive prices, we have work many times, every time is delighted, wish continue to maintain!
    5 Stars By Aurora from Russia - 2018.05.15 10:52
    Write your message here and send it to us