Super Lowest Price Polyvinyl Butyral Interlayer - Dark green on light green FG101 – Baizan

Short Description:


Product Detail

Related Video

Feedback (2)

Well-run equipment, professional sales team, and better after-sales services; We are also a unified big family, everyone stick to the company value "unification, dedication, tolerance" for Car Glass Film Protection, Rto Approved Glass Film, Stick On Safety Glass Film, We persistently develop our enterprise spirit "quality lives the business, credit score assures cooperation and retain the motto inside our minds: consumers very first.
Super Lowest Price Polyvinyl Butyral Interlayer - Dark green on light green FG101 – Baizan Detail:

Green on clear C102

Baizan 0.45mm pvb film dark green on light green for car glass
Product volume>12000t per year
Payment terms:TT LC DP
Delivery time:5-10days
After-sale service:We will follow customer’s testing result, and if there is a problem, we will check it out at site.

Head model impact test
Prepare six glass sheets with a size of 1100mm*500. The composite sheet was placed in 20±5℃ for 4 hours, then remove them in a designated position. Then the head model with a weight of 10kg±0.2g was vertically detached from the sample at a height of 1.5m. The test drop point should be located within a range of 40mm from the sample center. The middle layer is allowed to break, but the human head model cannot penetrate the sample without large debris stripping. Finally, if 4 samples or less than 4 samples meet the above requirements, they will be disqualified. If 5 samples meet the above requirements, 6 new samples will be added. If all 6 samples meet the above requirements, they will be qualified.

ttgtdgsdg

Heat resistance test
Turn on the drying oven and adjust the temperature to 100℃. Prepare a piece of glass with thickness 2 mm.
Put the glass sheets into a 100℃ constant temperature drying oven for 2 hours, then take them out and observe whether there are bubbles or white. Other defects such as bubbles and discoloration shall not occur on the part 15mm beyond the edge or 10mm beyond the crack

Moisture test
Instrument: Moisture meter.
Cut the sample 5g±0.005g and put into the metal plate of the tester. After the machine finish the determination, the moisture value is read

xvcvsdsd


Product detail pictures:

Super Lowest Price Polyvinyl Butyral Interlayer - Dark green on light green FG101 – Baizan detail pictures


Related Product Guide:

Using a complete scientific high quality management program, superior high quality and superior faith, we acquire great reputation and occupied this industry for Super Lowest Price Polyvinyl Butyral Interlayer - Dark green on light green FG101 – Baizan , The product will supply to all over the world, such as: Serbia, Los Angeles, Dubai, We guarantee that our company will try our best to reduce customer purchase cost , shorten the period of purchase , stable merchandise quality , increase customers' satisfaction and achieve win-win situation .
  • The customer service staff's answer is very meticulous, the most important is that the product quality is very good, and packaged carefully, shipped quickly!
    5 Stars By Hedy from kazakhstan - 2018.12.14 15:26
    The customer service staff is very patient and has a positive and progressive attitude to our interest, so that we can have a comprehensive understanding of the product and finally we reached an agreement, thanks!
    5 Stars By Mabel from New York - 2018.12.30 10:21
    Write your message here and send it to us